Тезис
PreviewISO 19403-2:2017 specifies a test method to measure the contact angle for the determination of the surface free energy of a solid surface. The method can be applied for the characterization of substrates and coatings.
NOTE 1 For the determination of the surface free energy of polymers and coatings, either the method in accordance with Owens, Wendt, Rabel and Kaelble or the method in accordance with Wu is used preferably.
NOTE 2 The morphological and chemical homogeneity have an influence on the measuring results.
NOTE 3 The procedures indicated in ISO 19403-2:2017 are based on the state-of-the-art employing the drop projection method in penumbral shadow. Other methods are not excluded.
NOTE 4 Measuring the contact angle on powders is not part of ISO 19403-2:2017. For further information, see the bibliography.
-
Текущий статус: ОпубликованоДата публикации: 2017-06
-
Версия: 1
-
- ICS :
- 01.040.87 Paint and colour industries (Vocabularies)
Приобрести данный стандарт
Формат | Язык | |
---|---|---|
std 1 92 | PDF + ePub | |
std 2 92 | Бумажный |
- CHF92
Жизненный цикл
-
Сейчас
ОпубликованоISO 19403-2:2017
Стандарт, который пересматривается каждые 5 лет
Этап: 90.92 (Будет пересмотрено)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00
-
Будет заменено
В стадии разработкиISO/DIS 19403-2
Появились вопросы?
Ознакомьтесь с FAQ
Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)