ISO 21028-2:2018 specifies the toughness requirements of metallic materials for use at temperatures between −20 °C and −80 °C to ensure their suitability for cryogenic vessels. This document is applicable to fine-grain and low-alloyed steels with specified yield strength ≤460 N/mm2, aluminium and aluminium alloys, copper and copper alloys and austenitic stainless steels.
NOTE For steel materials listed in EN 13445‑2 or EN 13480‑2 or for steel materials and weldings complying with the same fundamental safety requirements, the requirements for prevention of brittle fracture at low temperatures according to EN 13445‑2:2014, Annex B, method 2, or EN 13480‑2:2012, Annex B, method 2 can be applied.
Общая информация
-
Текущий статус: ОпубликованоДата публикации: 2018-03Этап: Подтверждение действия международного стандарта [90.93]
-
Версия: 2
-
Технический комитет :ISO/TC 220ICS :23.020.40
- RSS обновления
Жизненный цикл
-
Ранее
ОтозваноISO 21028-2:2004
-
Сейчас
ОпубликованоISO 21028-2:2018
Стандарт, который пересматривается каждые 5 лет
Этап: 90.93 (Подтверждено)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00